Feet Failure.
This looked okay, and I was optimistic about the potentiality.
But.... as I started to polish them something rather nasty started to reveal itself... an oversight that I should have considered; the perimeter of the #16 bonding agent became apparent... and rather unslightly.
Half-way through the polishing of the feet:
Meh... flaw is not so apparent:
...until viewed from the top:
Each of the aberations are inconsitencies in the lamination. The solution would have been to over-laminate, then cut within the #16 perimeter...
...live and learn.
So... now I am in the process of making 5 more feet, same profile but slightly different combination of laminations.