I've seen people who have had nickel plating on a Koolance Full Coverage Block get stripped because of silver, and I've seen nickel plating on fittings get ruined because of silver. It seems to be very prevalent in some situations and then these people like you guys who have absolutely no issues with it. Personally I'd rather be safe than sorry.

EK and Koolance both have plating issues aside from silver use,dont confuse the 2
MILSPEC II
(8 items)
 
| LUMO |
(6 items)
 
CLoS3 IMPACT
(8 items)
 
CPUMotherboardGraphicsGraphics
5820k X99m WS 980ti strix 980ti strix 
RAMHard DrivePowerCase
KLEVV Cras DDR4  3tb Red Corsair 600w SFX + 450w SFX Caselabs BH4 
CPUMotherboardGraphicsRAM
4970k Z97 Gryphon GTX 680 x2 Crucial Ballistix Elite 16Gb 
PowerCase
Be Quiet Dark Power 850 InWin D Frame Mini 
CPUMotherboardGraphicsRAM
i7 4770k ASUS Impact ITX R9 290 Gskill Trident 2400 
Hard DriveHard DriveCoolingCase
Samsung EV0 250 x2 WD black Loop.....oh yes...... Caselabs S3....modded 
  hide details  
Reply
MILSPEC II
(8 items)
 
| LUMO |
(6 items)
 
CLoS3 IMPACT
(8 items)
 
CPUMotherboardGraphicsGraphics
5820k X99m WS 980ti strix 980ti strix 
RAMHard DrivePowerCase
KLEVV Cras DDR4  3tb Red Corsair 600w SFX + 450w SFX Caselabs BH4 
CPUMotherboardGraphicsRAM
4970k Z97 Gryphon GTX 680 x2 Crucial Ballistix Elite 16Gb 
PowerCase
Be Quiet Dark Power 850 InWin D Frame Mini 
CPUMotherboardGraphicsRAM
i7 4770k ASUS Impact ITX R9 290 Gskill Trident 2400 
Hard DriveHard DriveCoolingCase
Samsung EV0 250 x2 WD black Loop.....oh yes...... Caselabs S3....modded 
  hide details  
Reply