i`m putting together an all copper w/c rig and was just wondering. will my fittings not still cause corrosion as there different metals
UVBOOM
(13 items)
 
  
CPUMotherboardGraphicsRAM
core 2 duo e6600 @ 3.8 ghz p5b deluxe wifi GTX260 4g xms 2 800 mhz 
Hard DriveOSMonitorPower
hitachi deathstar250 seagate barrcuda 250 Win7 Ult yep two o those hyper type R 600w 
Case
Sunbeamtech uv blue 
  hide details  
Reply
UVBOOM
(13 items)
 
  
CPUMotherboardGraphicsRAM
core 2 duo e6600 @ 3.8 ghz p5b deluxe wifi GTX260 4g xms 2 800 mhz 
Hard DriveOSMonitorPower
hitachi deathstar250 seagate barrcuda 250 Win7 Ult yep two o those hyper type R 600w 
Case
Sunbeamtech uv blue 
  hide details  
Reply
post #2 of 12
Not as long as you stick with brass fittings and nickel plated barbs.
  
Reply
  
Reply
post #3 of 12
Us some good coolent and you wont have to worry about that!
post #4 of 12
Quote:
Originally Posted by sublime0 View Post
Us some good coolent and you wont have to worry about that!
No coolant will prevent aluminum and copper from destroying eachother. however, barbs are not typically aluminum, so you should be fine.
Dark Helmet
(13 items)
 
  
CPUMotherboardGraphicsRAM
Q6600 G0 @ 3.4ghz, 1.39v DFI LP UT P35-T2R XFX 6970 4gb G.Skill PC8000, 2gb G.Skill PC8500 
Hard DriveOSMonitorKeyboard
OCZ Vertex 2 60gb, WD Black 1tb, Samsung F1 1tb Windows 7 x64 Samsung 206bw Razer Tarantula 
PowerCaseMouse
Seasonic X650 Antec P182 Razer DeathAdder 
  hide details  
Reply
Dark Helmet
(13 items)
 
  
CPUMotherboardGraphicsRAM
Q6600 G0 @ 3.4ghz, 1.39v DFI LP UT P35-T2R XFX 6970 4gb G.Skill PC8000, 2gb G.Skill PC8500 
Hard DriveOSMonitorKeyboard
OCZ Vertex 2 60gb, WD Black 1tb, Samsung F1 1tb Windows 7 x64 Samsung 206bw Razer Tarantula 
PowerCaseMouse
Seasonic X650 Antec P182 Razer DeathAdder 
  hide details  
Reply
post #5 of 12
Quote:
Originally Posted by Dryadsoul View Post
Not as long as you stick with brass fittings and nickel plated barbs.
No bare aluminum touching bare steel and you should be golden....brass/nickel or brass/aluminum is good too....Stay away from copper it reacts with alot of different metal....
 
Resurrection
(11 items)
 
 
CPUMotherboardGraphicsRAM
Intel i7 3820 @4.75 Asus Rampage IV Gene X79 EVGA GTX 670 FTW Signature 2 16Gb GSkill Ripjaw X 1600 @1666 
Hard DriveHard DriveHard DriveOptical Drive
Crucial M4 128Gb Seagate Barracuda ST1000DM003  Mushkin Chronos Enhanced Deluxe 60Gb Samsung BluRay drive 
CoolingOSMonitorKeyboard
Xigmatek Dark Knight 2 Nighthawk Edition Windows 7 Home Premium 64Bit Asus PA248Q Ideazon Merc Stealth 
PowerCaseMouseMouse Pad
Corsair AX-750 Coolermaster HAF Xb Mionix Naos 8200 X Trac Ripper XXL 
AudioOtherOther
Creative Labs Titanium Pro to Pioneer Amp Lamptron FC5V2 Fan Controller KLH 3-way 8-inch Bookshelves / Sennheiser HD-555 
CPUGraphicsHard DriveMonitor
Intel i7-4930K EVGA GTX 780 Crucial M500 960Gb Asus PB278Q 
  hide details  
Reply
 
Resurrection
(11 items)
 
 
CPUMotherboardGraphicsRAM
Intel i7 3820 @4.75 Asus Rampage IV Gene X79 EVGA GTX 670 FTW Signature 2 16Gb GSkill Ripjaw X 1600 @1666 
Hard DriveHard DriveHard DriveOptical Drive
Crucial M4 128Gb Seagate Barracuda ST1000DM003  Mushkin Chronos Enhanced Deluxe 60Gb Samsung BluRay drive 
CoolingOSMonitorKeyboard
Xigmatek Dark Knight 2 Nighthawk Edition Windows 7 Home Premium 64Bit Asus PA248Q Ideazon Merc Stealth 
PowerCaseMouseMouse Pad
Corsair AX-750 Coolermaster HAF Xb Mionix Naos 8200 X Trac Ripper XXL 
AudioOtherOther
Creative Labs Titanium Pro to Pioneer Amp Lamptron FC5V2 Fan Controller KLH 3-way 8-inch Bookshelves / Sennheiser HD-555 
CPUGraphicsHard DriveMonitor
Intel i7-4930K EVGA GTX 780 Crucial M500 960Gb Asus PB278Q 
  hide details  
Reply
post #6 of 12
Stay away from copper? =/

Erm, no. Stay away from aluminium.

Buy nickel plated barbs and don't use any aluminium blocks and you'll be fine
Main Rig
(13 items)
 
  
CPUMotherboardGraphicsRAM
Intel C2D E6700 Asus P5KPL-AM mATX Palit GTS250 2 x 2GB OCZ PC2-8500 
Hard DriveOptical DriveOSMonitor
Western Digital 500GB Pioneer DVD-RW Windows 7 Ultimate 64-bit Viewsonic VA2213w 
KeyboardPowerCaseMouse
Logitech Media Keyboard Deluxe 750W Thermaltake Toughpower Antec NSW4400 Logitech MX510 
  hide details  
Reply
Main Rig
(13 items)
 
  
CPUMotherboardGraphicsRAM
Intel C2D E6700 Asus P5KPL-AM mATX Palit GTS250 2 x 2GB OCZ PC2-8500 
Hard DriveOptical DriveOSMonitor
Western Digital 500GB Pioneer DVD-RW Windows 7 Ultimate 64-bit Viewsonic VA2213w 
KeyboardPowerCaseMouse
Logitech Media Keyboard Deluxe 750W Thermaltake Toughpower Antec NSW4400 Logitech MX510 
  hide details  
Reply
post #7 of 12
Quote:
Originally Posted by tehpwnerofn00bs View Post
No coolant will prevent aluminum and copper from destroying eachother. however, barbs are not typically aluminum, so you should be fine.

What I was thinking, but I am not up to date enough on coolants to chime in.....
 
Resurrection
(11 items)
 
 
CPUMotherboardGraphicsRAM
Intel i7 3820 @4.75 Asus Rampage IV Gene X79 EVGA GTX 670 FTW Signature 2 16Gb GSkill Ripjaw X 1600 @1666 
Hard DriveHard DriveHard DriveOptical Drive
Crucial M4 128Gb Seagate Barracuda ST1000DM003  Mushkin Chronos Enhanced Deluxe 60Gb Samsung BluRay drive 
CoolingOSMonitorKeyboard
Xigmatek Dark Knight 2 Nighthawk Edition Windows 7 Home Premium 64Bit Asus PA248Q Ideazon Merc Stealth 
PowerCaseMouseMouse Pad
Corsair AX-750 Coolermaster HAF Xb Mionix Naos 8200 X Trac Ripper XXL 
AudioOtherOther
Creative Labs Titanium Pro to Pioneer Amp Lamptron FC5V2 Fan Controller KLH 3-way 8-inch Bookshelves / Sennheiser HD-555 
CPUGraphicsHard DriveMonitor
Intel i7-4930K EVGA GTX 780 Crucial M500 960Gb Asus PB278Q 
  hide details  
Reply
 
Resurrection
(11 items)
 
 
CPUMotherboardGraphicsRAM
Intel i7 3820 @4.75 Asus Rampage IV Gene X79 EVGA GTX 670 FTW Signature 2 16Gb GSkill Ripjaw X 1600 @1666 
Hard DriveHard DriveHard DriveOptical Drive
Crucial M4 128Gb Seagate Barracuda ST1000DM003  Mushkin Chronos Enhanced Deluxe 60Gb Samsung BluRay drive 
CoolingOSMonitorKeyboard
Xigmatek Dark Knight 2 Nighthawk Edition Windows 7 Home Premium 64Bit Asus PA248Q Ideazon Merc Stealth 
PowerCaseMouseMouse Pad
Corsair AX-750 Coolermaster HAF Xb Mionix Naos 8200 X Trac Ripper XXL 
AudioOtherOther
Creative Labs Titanium Pro to Pioneer Amp Lamptron FC5V2 Fan Controller KLH 3-way 8-inch Bookshelves / Sennheiser HD-555 
CPUGraphicsHard DriveMonitor
Intel i7-4930K EVGA GTX 780 Crucial M500 960Gb Asus PB278Q 
  hide details  
Reply
post #8 of 12
Quote:
Originally Posted by prosser13 View Post
Stay away from copper? =/

Erm, no. Stay away from aluminium.

Buy nickel plated barbs and don't use any aluminium blocks and you'll be fine
I guess it's a preference....copper looks ugly when it oxidizes....
 
Resurrection
(11 items)
 
 
CPUMotherboardGraphicsRAM
Intel i7 3820 @4.75 Asus Rampage IV Gene X79 EVGA GTX 670 FTW Signature 2 16Gb GSkill Ripjaw X 1600 @1666 
Hard DriveHard DriveHard DriveOptical Drive
Crucial M4 128Gb Seagate Barracuda ST1000DM003  Mushkin Chronos Enhanced Deluxe 60Gb Samsung BluRay drive 
CoolingOSMonitorKeyboard
Xigmatek Dark Knight 2 Nighthawk Edition Windows 7 Home Premium 64Bit Asus PA248Q Ideazon Merc Stealth 
PowerCaseMouseMouse Pad
Corsair AX-750 Coolermaster HAF Xb Mionix Naos 8200 X Trac Ripper XXL 
AudioOtherOther
Creative Labs Titanium Pro to Pioneer Amp Lamptron FC5V2 Fan Controller KLH 3-way 8-inch Bookshelves / Sennheiser HD-555 
CPUGraphicsHard DriveMonitor
Intel i7-4930K EVGA GTX 780 Crucial M500 960Gb Asus PB278Q 
  hide details  
Reply
 
Resurrection
(11 items)
 
 
CPUMotherboardGraphicsRAM
Intel i7 3820 @4.75 Asus Rampage IV Gene X79 EVGA GTX 670 FTW Signature 2 16Gb GSkill Ripjaw X 1600 @1666 
Hard DriveHard DriveHard DriveOptical Drive
Crucial M4 128Gb Seagate Barracuda ST1000DM003  Mushkin Chronos Enhanced Deluxe 60Gb Samsung BluRay drive 
CoolingOSMonitorKeyboard
Xigmatek Dark Knight 2 Nighthawk Edition Windows 7 Home Premium 64Bit Asus PA248Q Ideazon Merc Stealth 
PowerCaseMouseMouse Pad
Corsair AX-750 Coolermaster HAF Xb Mionix Naos 8200 X Trac Ripper XXL 
AudioOtherOther
Creative Labs Titanium Pro to Pioneer Amp Lamptron FC5V2 Fan Controller KLH 3-way 8-inch Bookshelves / Sennheiser HD-555 
CPUGraphicsHard DriveMonitor
Intel i7-4930K EVGA GTX 780 Crucial M500 960Gb Asus PB278Q 
  hide details  
Reply
post #9 of 12
I wouldn't be too worried about it, unless you using a Swiftech Apogee GTX with an aluminum top you should be fine.

Ohh and the Fuzion v2 refers to the fact that it is the recently release second version of the Fuzion line.
    
CPUMotherboardGraphicsRAM
C2D T7100 1.8 ghz (undervolted) ummm... Dell Intel X3100 2 x 1gb 667mhz 
Hard DriveOptical DriveOSMonitor
Fujitsu 7200 RPM 120gb CD-RW/DVD dual boot Vista business 1440x900 
  hide details  
Reply
    
CPUMotherboardGraphicsRAM
C2D T7100 1.8 ghz (undervolted) ummm... Dell Intel X3100 2 x 1gb 667mhz 
Hard DriveOptical DriveOSMonitor
Fujitsu 7200 RPM 120gb CD-RW/DVD dual boot Vista business 1440x900 
  hide details  
Reply
post #10 of 12
Quote:
Originally Posted by Ramsey77 View Post
I guess it's a preference....copper looks ugly when it oxidizes....
Copper is what most blocks are made of now and is a much better heat conductor than aluminium...
Main Rig
(13 items)
 
  
CPUMotherboardGraphicsRAM
Intel C2D E6700 Asus P5KPL-AM mATX Palit GTS250 2 x 2GB OCZ PC2-8500 
Hard DriveOptical DriveOSMonitor
Western Digital 500GB Pioneer DVD-RW Windows 7 Ultimate 64-bit Viewsonic VA2213w 
KeyboardPowerCaseMouse
Logitech Media Keyboard Deluxe 750W Thermaltake Toughpower Antec NSW4400 Logitech MX510 
  hide details  
Reply
Main Rig
(13 items)
 
  
CPUMotherboardGraphicsRAM
Intel C2D E6700 Asus P5KPL-AM mATX Palit GTS250 2 x 2GB OCZ PC2-8500 
Hard DriveOptical DriveOSMonitor
Western Digital 500GB Pioneer DVD-RW Windows 7 Ultimate 64-bit Viewsonic VA2213w 
KeyboardPowerCaseMouse
Logitech Media Keyboard Deluxe 750W Thermaltake Toughpower Antec NSW4400 Logitech MX510 
  hide details  
Reply
New Posts  All Forums:Forum Nav:
  Return Home
  Back to Forum: Water Cooling
Overclock.net › Forums › Cooling › Water Cooling › galvanic corrosion