Same here, LET hasn't been an issue for me under LN2. I use Dragonskin all the time for Cascade benching since it seems fine up to about -140, approx. After that Dragonskin will start cracking if there isn't a buffer (I use a gasket of neoprene or Frost King foam) between the pot and the dragonskin. I've full pot benched using dragonskin with a gasket numerous times, without gasket it cracks around the socket. LET or eraser have both been fine.